Blog
Electroplating Thickness: Specify the Final Fit Before Ordering
Electroplating thickness can turn a passing machined shaft into an oversized fit or reduce the clearance in a bore. State whether critical dimensions apply before or after plating, then identify the coating, thickness limits and measurement locations. A note saying only “nickel plate” leaves too much unresolved.
Specify the actual coating process
Electrolytic nickel plating and electroless nickel are different processes. Do not treat their coating specifications or post-treatment requirements as interchangeable. The Nickel Institute handbook explains how current distribution and geometry influence electrolytic nickel thickness: projections and recessed areas can receive different deposits. Confirm the critical locations with the plater rather than assuming one uniform thickness over the whole component.
Budget for electroplating thickness at the fit
For a simple cylindrical surface with equal radial deposit thickness t, an outside diameter grows by approximately 2t; a fully coated bore diameter reduces by approximately 2t. This is a geometric estimate, not proof of uniform plating. As an illustrative calculation, 10 micrometers per side would change diameter by about 20 micrometers. Actual local thickness, preparation and any final finishing must be considered before setting machining targets.
| Drawing item | Instruction to resolve | Acceptance record |
|---|---|---|
| Critical fit | Final plated size and allowable thickness at the feature | Post-plating size and local thickness as specified |
| Masked surface | Boundary and permitted transition region | Inspection against the marked drawing |
| Recess or internal feature | Coverage and measurement access | Agreed location and suitable measurement method |
| Susceptible steel | Required embrittlement controls under the invoked specification | Applicable process records and tests |
Agree post-treatment requirements for the base material
As one application-specific example, NASA/JSC PRC-5007 Rev. E defines electroless nickel requirements including thickness callouts, thermal treatment classes and hydrogen-relief provisions for identified materials and conditions. It is not a universal recipe for electroplating. Use the contractually invoked current specification and material condition; do not copy a bake cycle from another alloy or part.
- Base material, condition and required coating specification.
- Significant surfaces, thickness limits and measurement locations.
- Before/after-plating dimensions, mask boundaries and final finish.
- Applicable relief, adhesion, corrosion or other acceptance requirements.
- Lot-linked coating records and final dimensional results.
Use the inspection report checklist to request the final evidence. The separate anodizing dimensional-change guide covers another finishing process; its growth behavior should not be substituted for deposited-metal calculations. Send the drawing and coating specification to tonyzhou@lxcet.com for an order-specific review.
The product photograph shows representative shaft fit surfaces; its coating process is not documented. Use the quality inspection overview when discussing which dimensional evidence is required for the order.